For standard cemented carbide, a graphite furnace is perfect. But for Titanium Alloys (TC4), Medical Implants, and Refractory Metals, graphite is the enemy.
At high temperatures, carbon atoms from graphite insulation can migrate and react with sensitive materials, forming brittle carbides (like TiC). For a hip joint implant or an aerospace turbine blade, this micro-contamination can lead to catastrophic fatigue failure.
To achieve medical-grade purity, you need an environment that is physically incapable of producing carbon. You need the Ruideer All-Metal Molybdenum Heating Furnace (RDE-Mo Series)
Designed for the most demanding applications in aerospace and healthcare, the RDE-Mo series replaces all carbon-based components with Molybdenum (Mo), Tungsten (W), and Stainless Steel.
Insulation: Instead of graphite felt, we use a multi-layered All-Metal Heat Shield (Molybdenum + Stainless Steel). It reflects heat efficiently without outgassing carbon or particles.
Heating Elements: Made of high-purity Molybdenum Strip or Mesh.
Benefit: Eliminates the risk of surface carburization ("Alpha Case"), ensuring your Titanium implants retain their superior biocompatibility and fatigue strength.
Metal hot zones do not absorb gases like graphite does.
Performance: This allows the furnace to reach a deeper vacuum level faster. While standard furnaces operate at 10-3 Pa, our RDE-Mo series can be upgraded to reach 10-4 Pa upon request.
Result: Minimizes oxygen and nitrogen pick-up, crucial for sintering reactive metals like Titanium and Niobium.
Temperature Control: Utilizing W-Re thermocouples and advanced PID control, we maintain strict temperature uniformity even at the maximum operating temperature of 1600°
Application: Perfect for sintering MIM Titanium parts (watch cases, surgical tools) and annealing refractory metals.
| Parameter | Specification |
|---|---|
| Max. Working Temperature | 1600°C |
| Hot Zone Material | Molybdenum / Stainless Steel (All-Metal) |
| Ultimate Vacuum | Standard: 10-3/ Optional: 10-4 Pa |
| Leakage Rate | 3 Pa/h (Average over 24h) |
| Cooling Time | < 5h - 7h (Rapid cooling available) |
| Standard Models |
RDE-4415-0Mo (400x400x1500mm) RDE-6612-0Mo (600x600x1200mm) |
Medical Implants: Titanium knee/hip joints, bone screws, dental implants.
Aerospace: Superalloy components, turbine blades.
Electronics: Refractory metal sintering (Tungsten/Molybdenum targets).
Luxury Goods: MIM Titanium watch cases and jewelry.
Don't compromise your material's integrity with the wrong furnace. Choose the Ruideer All-Metal Solution for absolute purity.
Contact us today to discuss your Titanium or Superalloy sintering requirements.
أرسل استفسارك مباشرة إلينا